Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 900 - 1100 MPa | 131000 - 160000 psi | |
Schmolz + Bickenbach UGICHROM 4418 Martensitic Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 930 - 1100 MPa | 135000 - 160000 psi | |
Schmolz + Bickenbach UGICHROM 4542 Martensitic Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 880 - 1100 MPa | 128000 - 160000 psi | 50<x=60mm |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength at Break | 880 - 1100 MPa | 128000 - 160000 psi | 60<x=80mm |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength at Break | 880 - 1100 MPa | 128000 - 160000 psi | 80<x=100mm |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength at Break | 940 - 1100 MPa @Thickness 50.0 mm |
136000 - 160000 psi @Thickness 1.97 in |
|
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength at Break | 970 - 1100 MPa | 141000 - 160000 psi | 50<x=60mm |
ThyssenKrupp XABO® 960 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength at Break | 650 - 1100 MPa | 94300 - 160000 psi | |
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy Information provided by Goodfellow. |