Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 560 - 720 MPa | 81200 - 104000 psi | |
ThyssenKrupp XABO® 500 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Tensile Strength at Break | 560 - 720 MPa | 81200 - 104000 psi | |
ThyssenKrupp XABO® 500 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Tensile Strength at Break | 530 - 720 MPa | 76900 - 104000 psi | |
ThyssenKrupp XABO® 460 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Tensile Strength at Break | 530 - 720 MPa | 76900 - 104000 psi | |
ThyssenKrupp XABO® 460 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |