Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.650 MPa | 94.3 psi | ASTM D3574 |
3M 4718 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Tensile Strength at Break | 0.650 MPa | 94.3 psi | Die "A"; ASTM D3759 |
3M 4718 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |