Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 632 MPa | >= 91700 psi | 7.2 lb. Minimum Tensile Load 0.01 in. Diameter |
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 6 lb 100% pure PVDF fluoro-polymer, great clarity, limpness and strength, low refractive index that decreases the visibility of the line.Information provided by Shakespeare Company. |