Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 62.0 MPa | 8990 psi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ E-PC CB Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments. Nemcon E-PC CB is a carbon black-filled polycarbonate characterized by consistent moldability, recyclability,.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY HRA170 ASA (Europe-Africa-Middle East) GELOY HRA170 is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour .. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 915R PC (Asia Pacific) Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties... |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East) Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML4588 PC Extrusion and extrusion blowmolding grade for aircraft applications. Meets FAR 25.853 (60 seconds/30 mils).This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | ASTM D638 |
LG Chemical LUCEL N145-02 General Purpose POM, Unreinforced, Externally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | ASTM D638 |
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | ASTM D638 |
LG Chemical LUCEL VC-145 Antistatic POM, Unreinforced, Ultra High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific) Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC (Asia Pacific) LNP* Stat-kon* DD0009E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X5500EX PBT+PC (Asia Pacific) Non-FR, non-UV PC/PBT blend for film extrusion application |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific) LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | ASTM D638 |
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | ISO 527-1/2 |
BLUESTAR BS130 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KFB11 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PFB91S PA 6 LNP* THERMOCOMP* PFB91S is a compound based on Nylon 6 resin containing Proprietary Filler(s). |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength at Break | 62.0 MPa | 8990 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East) CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha.. |