Polymer Property : Tensile Strength at Break = 876 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.04 MPa
876 psi
257°F, 70 hr in IRM 903 Oil; ASTM D471
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer
A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..