Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D412 |
Polimeri Europa Europrene® SOL T 6320 Styrene - Butadiene Block Copolymer Europrene® SOL T 6320 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 31% weight and diblock content is 75%. .. |
|||
Tensile Strength at Break | <= 6.00 MPa | <= 870 psi | ISO/R527 |
Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based Information provided by Polykemi AB |
|||
Tensile Strength at Break | 6.00 - 10.0 MPa | 870 - 1450 psi | |
Prodways PLASTCure Flex 100 3D Printing Polymer High workability. Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Suitable for the manufacture of flexible objects for.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D412 |
Teknor Apex Telcar® TL-1035-70UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ISO 527 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D412 |
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 502500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 602500S SEBS Based Material, Filled Qualities, 50A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 662550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer Product Description: UL 04331EL is a HEVA grade, especially designed for photovoltaic cells and encapsulation applications, requiring a good balance of adhesion and COF. It offers excellent light tr.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ISO 527-2/1A/50 |
ExxonMobil LDPE LD 655 Low Density Polyethylene Resin (European Grade) Product Description: LD 655 is a very high flow LDPE grade with a very good flexibility. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabiliz.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 600550S SEBS Based Material, Filled Qualities, 55A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate LOTRYL® 30 BA 02 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 30 BA 02 is used for polymer modification, in compounds formula.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4603 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure process in autoclave reactor. LOTADER 4603 is a multipurpose extrusion adhesive used.. |