Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 596 MPa | >= 86500 psi | 6 lb. Minimum Tensile Load 0.0094 in. Diameter |
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 6 lb Information provided by Shakespeare Company. |