Mechanical Properties Metric English Comments
Tensile Strength at Break 52.4 MPa
7600 psi
ASTM D638
Niche Polymer PA66HIBK Nylon 66, High Impact
Information provided by Niche Polymer
Tensile Strength at Break 52.4 MPa
7600 psi
ASTM D638
Niche Polymer PA66HIN Nylon 66, High Impact
Information provided by Niche Polymer
Tensile Strength at Break 52.4 MPa
7600 psi
Indium Corp. Indalloy 109 Tin-Lead Solder Alloy
Good electrical grade solderInformation Provided by Indium Corporation
Tensile Strength at Break 52.4 MPa

@Temperature 150 °C
7600 psi

@Temperature 302 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Tensile Strength at Break >= 52.4 MPa
>= 7600 psi
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Description: Master Bond Polymer System Supreme 11HT-LO is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room ..
Tensile Strength at Break 52.4 MPa
7600 psi
ASTM D638
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp
Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Tensile Strength at Break 52.4 MPa
7600 psi
ASTM D638
Entec Hyrene® PSCRY 1.5 General Purpose Polystyrene
Available in North America Features: Crystal, High Heat Resistance, General Purpose, High Molecular WeightRoHS Compliant Form: Pellets Information provided by Entec
Tensile Strength at Break 52.4 MPa
7600 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B9424-3 , 3% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Tensile Strength at Break 52.4 MPa

@Temperature 150 °C
7600 psi

@Temperature 302 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..