Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.80 MPa | 696 psi | Across flow; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength at Break | 4.80 MPa | 696 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant Product Description: A soft, black, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has been designed to meet the Underwriter Laboratories.. |
|||
Tensile Strength at Break | 4.80 MPa | 696 psi | chs 20 in/min; ASTM D412 |
Diamond Polymers Softflex® SF 7001 Thermoplastic Vulcanizate (TPV) Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength at Break | 4.80 MPa | 696 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 50 A.1 black TPE-S, Shore A50, black TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 4.80 MPa | 696 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 55 A.01 TPE-S, Shore A55, natural TPE-SInformation provided by BARLOG plastics GmbH. |