Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 44.0 MPa | 6380 psi | ASTM D638 |
Niche Polymer ABSN4BK ABS Information provided by Niche Polymer |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific) Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | ISO 527-2 |
Total Lacqrene® 1240 Crystal Polystyrene
(discontinued **) LACQRENE® 1240 is a high molecular weight crystal polystyrene, used in the dilution of high impact grades of polystyrene such as LACQRENE® 7240 or clear impact polystyrene such as Finaclear 520. .. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific) Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 50mm/min; ASTM D638 |
Kingfa FW-620 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | ISO R 527 |
Stir SpA RS 18 (PVC) Application: Molding for bends, connections and electrical fittings for buildingInformation provided by STIR SpA |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | ISO 527 |
Styrolution PS-145D Polystyrene Description: Polystyrene 145D is a high flow, general purpose polystyrene. PS 145D offers exceptional processing characteristics for thing walled parts, multi-cavity tools, and complex designs. It i.. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | ISO 527 |
Styron Pulse® 920 MG PC/ABS An inherently matt medium heat, medium impact PC/ABS resin, PULSE™ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro.. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | 50 mm/min; ISO 527 |
Eurostar Staramide PX08000 PA6, Impact Modified, Injection Molded Staramide PX08000 is an Impact Modified Polyamide 6 Injection Molding Resin (also known as Star X 2006)Information provided by Eurostar. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | ASTM D638 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | ASTM D412 |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |
|||
Tensile Strength at Break | 44.0 MPa | 6380 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |