Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 42.1 MPa | 6110 psi | 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength at Break | 42.1 MPa | 6110 psi | ASTM D412 |
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester Polyether-based grades for film and sheet applications that require excellent resistance to hydrolysis and microbial attack.Information provided by Alliance Polymers |
|||
Tensile Strength at Break | 42.1 MPa | 6110 psi | TD; ASTM D882 |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |