Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 414 MPa | 60000 psi | Stainless Steel (18-8) Annealed butt joint |
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet.. |
|||
Tensile Strength at Break | 414 MPa | 60000 psi | Annealed |
California Fine Wire Copper Clad 1006 Steel (40% Conductivity) All values may vary dependent on specific design and usage1006 steel core, 99.99% copper cladCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 414 MPa | 60000 psi | Annealed |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 414 MPa | 60000 psi | Hard |
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 414 MPa | 60000 psi | Annealed |
California Fine Wire Nico Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 414 MPa | 60000 psi | ACMA Test #4 / DIN EN 843-1 |
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 950 has a combination of high strength (from zirconia) and high hardness (from the alumina phase). It has excellent wear resistance, both in sliding and abrasive conditions. This material offers a g.. |
|||
Tensile Strength at Break | 414 MPa | 60000 psi | |
Mueller Ecostream™ C36500 Uninhibited Leaded Muntz Metal As one of the lower lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36500 alloy provides a viable alternative to those manufacturers who are manufacturing produc.. |