Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.10 MPa | 594 psi | Air at 212°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 281-45MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tensile Strength at Break | 4.10 MPa @Time 7200 sec |
594 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1050 TPE Product Description: StarCLEAR CLR-1050 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat.. |
|||
Tensile Strength at Break | 4.10 MPa @Time 7200 sec |
594 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1040 TPE Product Description: StarCLEAR CLR-1040 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat.. |