Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 38.3 MPa | 5550 psi | ASTM D638 |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Tensile Strength at Break | 38.3 MPa | 5550 psi | ASTM D3759 |
3M 3302 Specialty Foil Tape Aluminum foil tape. EMI/RFI shielding. Ul 510 Recognized.Information provided by 3M |