Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.35 MPa @Time 7200 sec |
486 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-55-1000 TPE Product Description: StarXTRUDE XTR-55-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |