Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 32.8 MPa | 4750 psi | ASTM D638 |
Amco Amalloy® B1172 Polymer Alloy Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials. |