Mechanical Properties Metric English Comments
Tensile Strength at Break 31.38 MPa
4551 psi
Taiwan PU Corporation TPU-B85 General Grade, Blow Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation.
Tensile Strength at Break 31.38 MPa
4551 psi
Taiwan PU Corporation TPU-BH90 Hydrolysis Resistance, Blow Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation.
Tensile Strength at Break 31.38 MPa
4551 psi
Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.