Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 360A4861316 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D3756 |
3M 201+ General Use Masking Tape 3M™ General Use Masking Tape 201+ is a tan colored crepe paper masking tape for holding, bundling, sealing, non-critical masking applications and a vast number of other jobs where a pressure sensit.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D3756 |
3M 200 Paper Tape 3M™ Paper Tape 200 is a utility purpose paper tape for holding, bundling, sealing, non-critical masking and a vast number of other jobs where a pressure-sensitive tape is needed.Information provide.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |