Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 25.4 MPa | 3680 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging XPL319 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of.. |
|||
Tensile Strength at Break | 25.4 MPa | 3680 psi | ASTM D638 |
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum Information provided by ITW Devcon |