Mechanical Properties Metric English Comments
Tensile Strength at Break 23.9 MPa
3460 psi
ASTM D412
Teknor Apex APEX® 2095-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi..