Mechanical Properties Metric English Comments
Tensile Strength at Break 235 MPa
34100 psi
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Tensile Strength at Break 235 MPa
34100 psi
ASTM D638
Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled
Information provided by Niche Polymer
Tensile Strength at Break 235 MPa

@Temperature 23.0 °C
34100 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide..
Tensile Strength at Break 235 MPa
34100 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance. - Natural: Ixef..
Tensile Strength at Break 235 MPa
34100 psi
ISO 527-1/-2
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Tensile Strength at Break 235 MPa
34100 psi
ISO 527-1/-2
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Tensile Strength at Break 235 MPa
34100 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber
Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good..
Tensile Strength at Break 235 MPa
34100 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go..
Tensile Strength at Break 235 MPa
34100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PF00DS PA 6 (Europe-Africa-Middle East)
LNP THERMOCOMP* PF00DS is a compound based on PA6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Strength at Break 235 MPa
34100 psi
ISO 527-93
Wellman Wellamid® GF1750-N2 50% Glass Fiber Reinforced Nylon 6
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Tensile Strength at Break 235 MPa
34100 psi
ISO 527-1/-2
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Tensile Strength at Break 235 MPa
34100 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GVL-5H nat PA*-GF50
Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na..
Tensile Strength at Break 235 MPa
34100 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45
Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a..
Tensile Strength at Break 235 MPa
34100 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m..
Tensile Strength at Break 235 MPa
34100 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN LT51G35HSLR BL661A Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Laser Weldable PPA High Performance Polyamide Information provided by DuPont Performance Polymers
Tensile Strength at Break 235 MPa
34100 psi
ISO 527
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Tensile Strength at Break 235 MPa
34100 psi
ISO 527
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural
Information provided by Eurotec®
Tensile Strength at Break 235 MPa

@Temperature 23.0 °C
34100 psi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102..
Copyright © lookpolymers.com All Rights Reserved