Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 23.3 MPa | 3380 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R148CE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 23.3 MPa | 3380 psi | ASTM D638 |
Resirene Resirene® 2220 Medium Impact Polystyrene Features:High FlowEasy ProcessingGood GlossHigh Tensile ModulusFDA Rating: 21 CFR 177.1640High ProductivityExternal LubricatedApplications:InjectionThin Wall ApplicationsHard to Fill MoldsHangersVid.. |
|||
Tensile Strength at Break | >= 23.3 MPa | >= 3380 psi | |
3M Controltac™ 8655C ES Changeable Graphic Film with Comply™ Adhesive 3M™ Controlact™ Plus Changeable Graphic Film with Comply™ Adhesive 8655C ES combines the features found in Controltac and Comply adhesive technologies, including pressure activation, positionabil.. |
|||
Tensile Strength at Break | 23.3 MPa | 3380 psi | ASTM D3759 |
3M Scotch® 8896 Strapping Tape Scotch® Strapping Tape 8896 is a high-performance clean-removal tape with a tensilized polypropylene film backing and pressure-sensitive adhesive. The tape is designed to secure appliance parts and.. |
|||
Tensile Strength at Break | 23.3 MPa | 3380 psi | |
3M Scotchcal™ IJ355%-10 Changeable Graphic Film 4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-sensitive adhesive; Changeable for clean removable without heat or chemicalsInformation provided by 3M |
|||
Tensile Strength at Break | >= 23.3 MPa | >= 3380 psi | |
3M Controltac™ 3500C Changeable Graphic Film with Comply™ Adhesive 4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast, easy, bub.. |
|||
Tensile Strength at Break | 23.3 MPa | 3380 psi | ASTM D3759 |
3M Scotch® 8898 Strapping Tape Scotch® Strapping Tape 8896 is a ge3neral-purpose tape with a tensilized polypropylene film backing and pressure-sensitive adhesive. The tape is designed for a wide variety of industrial and packag.. |
|||
Tensile Strength at Break | 23.3 MPa | 3380 psi | ASTM D3574 |
3M 477 Vinyl Tape 3M™ Vinyl Tape 477 is comprised of a conformable, transparent vinyl backing with a versatile rubber adhesive. It is an excellent tape to use where abrasion resistance, transparency, conformability .. |
|||
Tensile Strength at Break | 23.3 MPa | 3380 psi | ASTM D638 |
Chesterton ARC CS2 Low-viscosity, Composite concrete primer sealer Description: An advanced composite formulated to protect concrete surfaces from mild chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat. Non-shrinking. 1.. |