Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 23.2 MPa @Temperature 100 °C, Time 605000 sec |
3370 psi @Temperature 212 °F, Time 168 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 7202 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 23.2 MPa | 3370 psi | ASTM D638 |
Teknor Apex APEX® 280-NL Polyvinyl Chloride, Flexible Notes: 75°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 23.2 MPa | 3370 psi | ASTM D638 |
Teknor Apex APEX® 3800-90 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |