Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 20.1 MPa @Temperature 200 °C, Time 252000 sec |
2910 psi @Temperature 392 °F, Time 70.0 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 7182D Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 20.1 MPa | 2910 psi | ASTM D412 |
Teknor Apex APEX® 3090-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |