Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2000 MPa | 290000 psi | |
ThyssenKrupp XAR® EXTRA Structural Steel This Material Specification applies to 4 to 40 mm thick plates of the wear-resistant special structural steel XAR® EXTRA. The high resistance to abrasion of XAR® EXTRA results from a special wate.. |
|||
Tensile Strength at Break | 2000 MPa | 290000 psi | |
ThyssenKrupp SECURE 600 Structural Steel This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 600 for civil use, that is usually produced from 4 up to 40 mm in thickness.Applic.. |
|||
Tensile Strength at Break | 2000 MPa | 290000 psi | |
ThyssenKrupp XAR® 600 Structural Steel This Material Specification applies to 4 to 40 mm thick plates of the wear-resistant special structural steel XAR® 600. The extraordinary high resistance to abrasion of XAR® 600 results from a sp.. |
|||
Tensile Strength at Break | 2000 MPa | 290000 psi | filament 25.4mm |
3M Nextel™ CF-40 Woven Fabric 550 Information provided by 3M |
|||
Tensile Strength at Break | 2000 MPa | 290000 psi | filament 25.4mm |
3M Nextel™ BF-30 Woven Fabric 440 Information provided by 3M |
|||
Tensile Strength at Break | 2000 MPa | 290000 psi | filament 25.4mm |
3M Nextel™ BF-20 Woven Fabric 440 Information provided by 3M |
|||
Tensile Strength at Break | 2000 MPa | 290000 psi | filament 25.4mm |
3M Nextel™ BF-40 Woven Fabric 440 Information provided by 3M |