Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 19.759 MPa | 2865.8 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |