Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 195 MPa | 28300 psi | |
Plastcom SLOVAMID 6/66 GF 30 FRG 5 TS PA6/66, 30% glass fibre, flame retardant FeaturesPA 6 + PA 66 alloy for injection moulding, chemically reinforced with 30 % glass fibre, with halogen and phosphorus free flame retardant. Main features: flammability in accordance with UL 94.. |
|||
Tensile Strength at Break | <= 195 MPa | <= 28300 psi | ISO/R527 |
Polykemi AB SCANAMID 66 A12^ F35 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | d.a.m.; ISO 527-1, -2; 5 mm/min |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | d.a.m.; ISO 527-1, -2; 5 mm/min |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO 527-1, -2; 5 mm/min |
Lanxess Durethan® BKV 40H2.0 EF 900116 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO 527 Type 1A |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO 527 Type 1A |
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, DRY Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors .. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXQ PA 66 LNP THERMOCOMP* RF007SXQ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Hydrolysis Resistant. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV007SX9 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV007SX9 is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AG-30 H PA66 Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor.. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-35/4 PA666-GF35 Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo.. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR55G50NHLW BK046 Polyphthalamide (PPA)
(Unverified Data**) 55% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Low Warpage and High Stiffness Zytel HTNFR55G50NHLW BK046 is a 50% glass reinforced flame retardant high perf.. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO 527 |
Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | 0.2 in/min; ASTM Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO 527-1/-2 |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO 527-93 |
Wellman Wellamid® GF33AO99 HR 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66 Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Tensile Strength at Break | 195 MPa | 28300 psi | ISO R 527 |
Addiplast Addinyl B2 ZV40 Nylon 6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |