Polymer Property : Tensile Strength at Break = 2830 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.5 MPa
2830 psi
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 90042 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Tensile Strength at Break 19.5 MPa
2830 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 90072 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 19.5 MPa
2830 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 90071 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 19.5 MPa
2830 psi
ASTM D412
Huntsman IROGRAN® PS 456-202 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Tensile Strength at Break 19.5 MPa
2830 psi
AVG; ASTM D412 Method A
Seals Eastern Perflas® 9294 Perfluorinated Rubber
Perfluoro rubber for aggressive chemical service. Perflas ® 9294 seals are made of a chemical resistant perfluorinated fluoroelastomer (FFKM). Perflas 9294 seals offer outstanding resistance to..
Tensile Strength at Break >= 19.5 MPa
>= 2830 psi
Sibur SKD-ND 2nd Group Butadiene Rubber (BR)
Buna CB 24. It is used in tires and the rubber and asbestos technical industries. It is combined with natural butadiene-styrene rubbers in any ratio, which is very important during production of a..
Tensile Strength at Break 19.5 MPa
2830 psi
3M Scotchkote™ EG 515 Urethane Ceramic Rebuild
Scotchkote Urethane Ceramic Rebuild EG 515 has been specifically developed as a 100% solids repair system with a degree of flexibility for rebuilding and resurfacing equipment operating in fluid flo..
Tensile Strength at Break 19.5 MPa
2830 psi
3M Scotchkote™ FG 514 Urethane Ceramic Lining
Scotchkote Urethane Ceramic Lining FG 514 has been specifically developed as a 100% solids polyceramic coating with a degree of flexibility for lining and resurfacing equipment operating in fluid fl..