Polymer Property : Tensile Strength at Break = 276000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1900 MPa
276000 psi
SGL Carbon Group SIGRAFIL C® in 250°F Epoxy
60% fiber volumeInformation provided by SGL Carbon Group
Tensile Strength at Break 1900 MPa
276000 psi
ASTM C297
3M RPF-CWR (0.417 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass with Woven Roving
3M™ RPF-C (Reinforced Polyurethane Foam) is a polyurethane foam with layers of continuous strand fiberglass and woven roving throughout the polyurethane. The composites are 30% to 45% lighter than ..