Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JAC32A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2180 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180 is a 80 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2180 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2180G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180G is a 80 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2180G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 3180G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 3180G is a non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 3180G can be used for extrusion and injection molding healthcare applications. This pr.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A9001 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A90U2 Polyvinyl Chloride, Flexible (PVC, Flexible) GENERAL PURPOSE CLEAR PVC COMPOUND WITH LOW LEVEL OF U.V. INHIBITOR, to be used only in interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV 3432 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This product has received full compliance certification for USP Biological Reactivity Tests under USP Plastic Class VI.NOTE: All ingredients used in the formulation of this compound are listed in th.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3887 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R235AE White 1875 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R363MB White 1876 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D4894 |
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 4107 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 77-W280B-9 Polyvinyl Chloride, Flexible Notes: 60°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 84459 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; Low to no Migration; Oil ResistantUses: Insulation Agency Ratings: UL 1063; UL 62; UL 1581 Forms: Pellets Wire Types: AWMInforma.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D412 |
Teknor Apex MF 165 NT Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D412 |
Teknor Apex Telcar® TL-101 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | PVC (70)/CP80AS2(30) |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Bayshore Vinyl Compounds BVC 4200-90 Vinyl Compound Information Provided by Bayshore Vinyl Compounds Inc. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R350AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Chase Plastics CP Pryme® PPC100-20M Polypropylene Copolymer Information provided by Chase Plastics. |