Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 172 - 207 MPa | 25000 - 30000 psi | Copper butt joint |
Lucas-Milhaupt BRAZE 250 Silver Based Cadmium Free Filler Metal Characteristics:Braze 250 is an intermediate temperature silver brazing alloy with a long (325EF/180EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting constitu.. |
|||
Tensile Strength at Break | 172 - 207 MPa | 25000 - 30000 psi | Copper butt joint |
Lucas-Milhaupt BRAZE 450 Silver Based Cadmium Free Filler Metal Characteristics:Braze 450 is an intermediate temperature cadmium free silver brazing filler metal with sufficient melting range (145EF) to properly braze joints with the range of fits encountered in.. |
|||
Tensile Strength at Break | 172 - 207 MPa | 25000 - 30000 psi | Copper butt joint |
Lucas-Milhaupt BRAZE 600 Silver Based Cadmium Free Filler Metal Characteristics: Braze 600 is a copper rich eutectiferous alloy, the eutectiferous portion of which is molten at 1300EF (705EC), about 25EF before the entire composition is completely fluid. Thus t.. |
|||
Tensile Strength at Break | 172 - 241 MPa | 25000 - 35000 psi | Brass butt joint |
Lucas-Milhaupt BRAZE 750 (Hard) Silver Based Cadmium Free Filler Metal Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel.. |
|||
Tensile Strength at Break | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES Electrafil® J-1305/CF/20 PPS |
|||
Tensile Strength at Break | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 NAT PPS |
|||
Tensile Strength at Break | 172 MPa | 25000 psi | ASTM D638 |
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Tensile Strength at Break | 172 MPa | 25000 psi | ASTM D638 |
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 BK2989 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Tensile Strength at Break | 172 MPa | 25000 psi | ASTM D638 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 BK223 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Tensile Strength at Break | 172 MPa | 25000 psi | ASTM D638 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 NAT PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |