Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WJLC32L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | ASTM D638 |
S&E Specialty Polymers TufFill NH™ 2102A PP, Flame Retardant Application: A polypropylene based, zero halogen, flame retardant compound with antistatic properties designed for packaging applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 1240 UV RoHS NATURAL Polyethylene, Chlorinated (CPE) An excellent choice for low-voltage power-and-cable control cables, this RoHS compliant filled, flexible thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantages of th.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8501 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A85UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible P1500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 86479 Natural Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 86479 Opaque Polyvinyl Chloride Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 86479 Tran Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B8502 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R323AE Polyvinyl Chloride Elastomer (PVC Elastomer) Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R328BE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | ISO 37 |
Alliance Polymers Viprene™ P55D-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P55D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | ISO 37 |
Alliance Polymers Viprene™ P55D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P55D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | |
3M HDT Heat Shrink Tubing 3M Heat Shrink Tubing HDT is a designed to provide reliable performance as well as excellent mechanical and environmental protection. This flame-retardant product combines the important advantage of.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | ASTM D412 |
3M Scotch® 31 Heavy Duty Mining Tape Scotch® Heavy Duty Mining Tape 31 has a tough, abrasion-resistant backing for jacket repair on mining cables. Due to extremely abrasive environment, the original jacket on the cable gets damaged of.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | ASTM D412 |
3M Scotch™ 2234 Cable Jacket Repair Tape 3M™ Scotch™ Cable Jacket Repair Tape 2234 provides a cost effective and efficient means of covering and protecting damaged sections of cable jacket, thereby extending the life of the cable and red.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | |
3M Scotch® FP-301 Heat Shrink Tubing Scotch® Heat Shrink Tubing FP-301 offers an outstanding balance of electrical, physical and chemical properties for a wide variety of industrial and military applications. Rated for 135°C continuo.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | |
3M Scotch® FP-301VW Heat Shrink Tubing Scotch® Heat Shrink Tubing FP-301VW has the same outstanding balance of electrical, physical and chemical properties as FP-301 tubing, and is specially engineered for excellent flame resistance. FP.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | |
3M MDT Tubing 3M MDT Tubing offers increased flexibility in combination with excellent abrasion, corrosion and environmental resistance properties and meets MIL-DTL-23053/15, Class 2. Uncoated product (without se.. |
|||
Tensile Strength at Break | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Syncure™ S1060A Polyethylene, Crosslinked (XLPE) Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1060A / 5 phr S1.. |