Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.59 MPa @Time 7200 sec |
231 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-1000 TPE Product Description: StarGrip GP 25-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
Tensile Strength at Break | 1.59 MPa @Temperature 60.0 °C |
231 psi @Temperature 140 °F |
JRF-14 days |
3M AC-350 Class A-1 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Tensile Strength at Break | 1.59 MPa @Temperature 60.0 °C |
231 psi @Temperature 140 °F |
JRF-14 days |
3M AC-350 Class A-1/2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Tensile Strength at Break | 1.59 MPa @Temperature 60.0 °C |
231 psi @Temperature 140 °F |
JRF-14 days |
3M AC-350 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Tensile Strength at Break | 1.59 MPa @Temperature 336 °C |
231 psi @Temperature 637 °F |
MIL-PRF-81733 AND AS5127A |
3M AC-736 B-2 Aerospace Sealant 3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an .. |
|||
Tensile Strength at Break | 1.59 MPa @Time 605000 sec |
231 psi @Time 168 hour |
180°F (82°C) and then tested at 75°F (24°C) |
3M Weatherban™ 606NF Acrylic Sealant 3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M.. |