Tensile Strength at Break 1.48 MPa

@Temperature 60.0 °C
215 psi

@Temperature 140 °F
JRF-14 days
3M AC-236 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Tensile Strength at Break 1.48 MPa

@Temperature 60.0 °C
215 psi

@Temperature 140 °F
JRF-14 days
3M AC-236 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Tensile Strength at Break 1.48 MPa
215 psi
JRF-12 days @ 60°C + 60 hrs @ 71°C + 6 hrs 82°C; AMS3276
3M AC-275 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Tensile Strength at Break 1.48 MPa
215 psi
JRF-12 days @ 60°C + 60 hrs @ 71°C + 6 hrs 82°C; AMS3276
3M AC-275 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Tensile Strength at Break 1.48 MPa
215 psi
JRF-12 days @ 60°C + 60 hrs @ 71°C + 6 hrs 82°C; AMS3276
3M AC-275 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Tensile Strength at Break 1.48 MPa
215 psi
3M Weatherban™ 606NF Acrylic Sealant
3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M..
Tensile Strength at Break 1.48 MPa

@Temperature 60.0 °C
215 psi

@Temperature 140 °F
JRF-14 days
3M AC-236 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..