Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1320 MPa | 191000 psi | |
Bisalloy Steels BisPlate 400 Thickness >80-100 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |
|||
Tensile Strength at Break | 1320 MPa | 191000 psi | |
Bisalloy Steels BisPlate 400 Thickness 5 - A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |
|||
Tensile Strength at Break | 1320 MPa | 191000 psi | |
Bisalloy Steels BisPlate 400 Thickness 16-80 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |