Mechanical Properties Metric English Comments
Tensile Strength at Break >= 1.24 MPa
>= 180 psi
ASTM D412
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer
Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie..
Tensile Strength at Break >= 1.24 MPa
>= 180 psi
ASTM D412
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material
Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in..
Tensile Strength at Break >= 1.24 MPa
>= 180 psi
ASTM D412
Parker Chomerics CHO-SEAL 1485 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Tensile Strength at Break 1.24 MPa
180 psi
ASTM D638
ExxonMobil ENABLE™ EN 33330 Adhesive Resin  (discontinued **)
Enable EN 33330 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.Information provided by ExxonMobil Chemical
Tensile Strength at Break >= 1.24 MPa
>= 180 psi
Base Material; ASTM D412
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..
Tensile Strength at Break 1.24 MPa
180 psi
ASTM D412
Teknor Apex Monprene® MP 2313 Thermoplastic Elastomer
Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly..
Tensile Strength at Break 1.24 MPa
180 psi
ASTM D412
Teknor Apex Monprene® MP-1880 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 1.24 MPa
180 psi
ASTM D638
ExxonMobil EN 33330 Ethylene n-Butyl Acrylate Copolymer Resin
Product Description: ExxonMobil EN 33330 is a high flow 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants. Availability: Latin America, North America and South America Additive..
Tensile Strength at Break 1.24 MPa
180 psi
Abatron MasterMold 12-3 Flexible Mold Making Compound
Master mold 12-3 is formulated for versatility, high elasticity and strength. It is a 2-component polyurethane system and can be easily spread on any model to produce a smooth bubble-free mold surf..
Tensile Strength at Break 1.24 MPa
180 psi
3M 4026 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Tensile Strength at Break >= 1.24 MPa
>= 180 psi
ASTM D412
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer
Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p..