Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.9 MPa | 1720 psi | Data derived from Type IV specimen, 75 mil plaques, @ 20" min.; ASTM D638 |
LyondellBasell Petrothene® NA143063 Low Density Polyethylene ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration.. |
|||
Tensile Strength at Break | 11.9 MPa | 1720 psi | |
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation |
|||
Tensile Strength at Break | 11.9 MPa | 1720 psi | Across flow; ASTM D412 |
ExxonMobil Santoprene® 8271-80HT Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use. It can be processed using injection molding or extrusion melt pro.. |