Mechanical Properties Metric English Comments
Tensile Strength at Break 11.8 MPa
1710 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 90450 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Tensile Strength at Break 11.8 MPa

@Thickness 2.00 mm
1710 psi

@Thickness 0.0787 in
50mm/min; ASTM D638
LG Chemical KEYFLEX BT GN7142F Ester Type TPE
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical
Tensile Strength at Break >= 11.8 MPa
>= 1710 psi
Sibur DST-45 RM Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE)
Kraton D 4271. For production of footwear compositions.
Tensile Strength at Break >= 11.8 MPa
>= 1710 psi
after aging (168h, 150°C); ASTM D412
Borealis PC0787 Polyethylene Insulation Compound, Crosslinkable
PC0787 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0787 contains flame retardant additives to reduce normal flame spread characteristics so as to achieve a..
Tensile Strength at Break 11.8 MPa
1710 psi
ISO 37
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 11.8 MPa
1710 psi
ISO 37
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer