Tensile Strength at Break 900 - 1050 MPa
131000 - 152000 psi
Schmolz + Bickenbach UGICHROM 4057 Martensitic Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength at Break 900 - 1100 MPa
131000 - 160000 psi
Schmolz + Bickenbach UGICHROM 4418 Martensitic Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength at Break 900 - 1050 MPa
131000 - 152000 psi
80<x=100mm
ThyssenKrupp XABO® 960 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Tensile Strength at Break 900 - 1200 MPa
131000 - 174000 psi
Longitudinal
Goodfellow Carbon/Vinyl Ester Rod
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Tensile Strength at Break 900 - 1200 MPa
131000 - 174000 psi
Longitudinal
Goodfellow Carbon/Vinyl Ester Tube
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Tensile Strength at Break 900 MPa

@Temperature 200 °C
131000 psi

@Temperature 392 °F
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy
UDIMET® alloy L-605 (UNS R30605) is a solid solution strengthened cobalt-chromium-tungsten-nickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°..
Copyright © lookpolymers.com All Rights Reserved