Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.38 MPa @Temperature 23.0 °C |
1070 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen.. |
|||
Tensile Strength at Break | 7.38 MPa @Time 7200 sec |
1070 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 55-HR-9 TPE Product Description: StarTUFF TF 55-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tensile Strength at Break | 7.40 MPa | 1070 psi | ASTM D412 |
Sumitomo Chemical ESPOLEX® WT485 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tensile Strength at Break | 7.40 MPa | 1070 psi | ISO 527 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 7.40 MPa | 1070 psi | ISO 527 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 7.40 MPa | 1070 psi | ISO 527 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 7.40 MPa | 1070 psi | ISO 527 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 7.40 MPa | 1070 psi | ISO 527 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 7.40 MPa | 1070 psi | ISO 527 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength at Break | 7.38 MPa | 1070 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-67W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Tensile Strength at Break | 7.38 MPa | 1070 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-79W233 Thermoplastic Elastomer A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner .. |
|||
Tensile Strength at Break | 7.40 MPa | 1070 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX E 75.1 TPE-V, Shore A75 TPE-VInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 7.38 MPa | 1070 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | 7.38 MPa | 1070 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |