Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 717 MPa | 104000 psi | Annealed |
Special Metals NILO® 365 Controlled-Expansion Alloy For the manufacture of tooling for composites, the NILO® nickel-iron alloys offer a unique combination of matched thermal expansion to avoid warping during the curing cycle, along with strength, .. |
|||
Tensile Strength at Break | 718 MPa @Temperature 760 °C, Time 3.60e+6 sec |
104000 psi @Temperature 1400 °F, Time 1000 hour |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |