Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.20 MPa | 1040 psi | ISO 37 |
PolyOne OnFlex™ S EF 60A-3S1967 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tensile Strength at Break | 7.20 MPa | 1040 psi | ISO 37 |
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tensile Strength at Break | 7.20 MPa | 1040 psi | ISO R 527 |
Stir SpA E 2092 65 (PVC) Application: Extrusion for seals and profilesInformation provided by STIR SpA |
|||
Tensile Strength at Break | 7.17 MPa | 1040 psi | ASTM D412 |
Teknor Apex APEX® 1519-39 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company |
|||
Tensile Strength at Break | 7.17 MPa | 1040 psi | ASTM D638 |
Teknor Apex Telcar® 90-E607B-75NT Ethylene Vinyl Acetate Copolymer Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several.. |
|||
Tensile Strength at Break | 7.17 MPa | 1040 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4876N Thermoplastic Elastomer Uses: Flexible Grips; Overmolding; Soft Touch Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Tensile Strength at Break | 7.17 MPa | 1040 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7100-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 7.20 MPa | 1040 psi | ISO 37 |
ELASTO UK Dryflex® 5049-110 TPE, Modified Injection Molding Grade for Auto Mud Flaps The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5049-110 is specifically designe.. |
|||
Tensile Strength at Break | 7.20 MPa | 1040 psi | ASTM D638 |
ELASTO UK Dryflex® 650450 TPE, Improved Compression Set and High Temperature Resistance, 45A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
Tensile Strength at Break | 7.17 MPa | 1040 psi | ISO 37 |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 7.17 MPa | 1040 psi | ISO 37 |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 7.18 MPa | 1040 psi | Longitudinal; ASTM D3759 |
3M Scotch® 681 Transparent Film Tape Scotch® Tape 681 is an excellent high tack, transparent film tape used for various packaging applications such as temporary holding, combining, light-duty carton sealing, bag sealing, and attaching.. |
|||
Tensile Strength at Break | 7.16 MPa | 1040 psi | ASTM D412 |
3M Scotchcast™ 2131 Flame-Retardant Compound 3M Scotchcast Flame-Retardant Compound 2131 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. It formulation makes it particu.. |
|||
Tensile Strength at Break | 7.17 MPa | 1040 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 181-64MED Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. .. |
|||
Tensile Strength at Break | 7.17 MPa | 1040 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-60W261 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |