Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.03 MPa | 1020 psi | ASTM D412 |
Multibase TPSiV™ 3040-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tensile Strength at Break | 7.03 MPa @Temperature 23.0 °C |
1020 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Tensile Strength at Break | <= 7.00 MPa | <= 1020 psi | ISO/R527 |
Polykemi AB POLYelast TPE ZS706 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
ICO Polymers ICOTEXâ„¢ 520-5004 1000 Micron EVA Powder Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a viny.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | Dry |
Kraton® NEXAR™ MD9200 Polymer Barrier Membrane NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification a.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ISO 527/2 |
Iran Petrochemical (PCC) 1922T Low Density Polyethylene LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Co.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
ELASTO UK Dryflex® 502600S SEBS Based Material, Unfilled Qualities, 60A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
ELASTO UK Dryflex® 600650S SEBS Based Material, Filled Qualities, 65A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
ELASTO UK Dryflex® 602600S SEBS Based Material, Filled Qualities, 60A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
ELASTO UK Dryflex® 660650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ISO R 527 |
Fainplast Compounds GS 55/T Flexible PVC, Injection Molding for Footwear Soles |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
Arkema Group LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate LOTRYL® 28 MA 07 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 28 MA 07 is a polyme.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (10 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Strength at Break | 7.00 - 10.0 MPa | 1020 - 1450 psi | ISO 527-1 |
Adamas Adalon® 452 PTFE, Mica filler Information provided by Adamas, HPM |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 65 A.01 TPE-S, Shore A65, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
Arkema Group EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate EVATANE® 40-55 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. It’s stabilized with antioxidants and contains slip and antiblock additiv.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |
|||
Tensile Strength at Break | 7.00 MPa | 1020 psi | ASTM D638 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |