Polymer Property : Tensile Strength at Break = 930 MPa
Polymer Property :
Tensile Strength at Break =
930 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
460
-
930
MPa
66700
-
135000
psi
Goodfellow Platinum 70/Rhodium 30 Thermocouple Alloy