Tensile Strength at Break 88.0 - 90.0 MPa
12800 - 13100 psi
ISO.527 DN.53455
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high..
Tensile Strength at Break 88.0 - 90.0 MPa
12800 - 13100 psi
ISO.527 DN.53455
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high..
Tensile Strength at Break 28.0 - 90.0 MPa
4060 - 13100 psi
ASTM D683
Loxim 811 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Tensile Strength at Break 88.0 - 90.0 MPa
12800 - 13100 psi
DIN 53455
Zell-Metall Engineering Plastics Zellamid 1100
Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers ..