Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 655 - 827 MPa | 95000 - 120000 psi | |
ThyssenKrupp X8Ni9 Structural Steel Data applies to plate thicknesses from 13/64 to 1 15/64 in.9% nickel steel for low temperature service down to -320°FApplication for pressure vessels and tanks for the transportation and storage of.. |