Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 34.5 - 75.8 MPa | 5000 - 11000 psi | Compared to 300 for concrete |
Abatron AboJet Structural Crack-Injection Resin Structural crack injection resin for foundations, dikes, columns, load-bearing walls and structures. Offers strength, performance, durability, cost effectiveness and restoration instead of demoliti.. |