Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.00 - 5.00 MPa | 435 - 725 psi | ASTM D412 |
Proto3000 Objet Digital Materials™ DM_9120/9420/9220/9320 Rubber-like Prototyping Polymer Primary material: TangoBlackSecondary material: VeroWhitePlus, VeroBlue, VeroBlack, FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific concen.. |
|||
Tensile Strength at Break | 3.00 - 5.00 MPa | 435 - 725 psi | ASTM D415 |
Proto3000 Objet TangoGray FullCure950 Rubber-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Tensile Strength at Break | 3.00 - 5.00 MPa | 435 - 725 psi | DIN 53504 S2 |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |