Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1200 - 1500 MPa | 174000 - 218000 psi | |
ThyssenKrupp XABO® 1100 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 4 up to 40 mm in thickness, made of the high-strength special structural steel XABO® 1100.Application: The stee.. |